Dow Corning SYL-OFF® 23-30% COATING

Category Fluid , Solvent
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® 23-30% COATING.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Syl-Off® 23 Paper Coating 30 Percent is a 30% active solids dispersion of silanol functional silicone polymers and multifunctional crosslinkers in xylene.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc

@Temperature 25.0 °C
0.900 g/cc

@Temperature 77.0 °F
Kinematic Viscosity 30000 cSt
30000 cSt
Storage Temperature <= 50.0 °C
<= 122 °F
Thermal Properties Metric English Comments
Flash Point 26.0 °C
78.8 °F
closed cup
Descriptive Properties Value Comments
Active Content (%) 30
Appearance clear liquid
Color slightly hazy
Solvent xylene
Users viewing this material also viewed the following: