Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 10% Igepal® | 20 hour | 20 hour | F50; ASTM D1963B |
ExxonMobil HDPE HD 6605.70 High Density Polyethylene Copolymer Resin Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan.. |
|||
ESCR 10% Igepal® | 20 hour | 20 hour | F50; ASTM D1963 |
ExxonMobil HDPE HYA 600 High Density Polyethylene Resin Product Description: HYA 600 is a general purpose HDPE resin, characterized by very easy processability, an excellent balance of rigidity and impact strength and a good ESCR.Availability: Africa & M.. |
|||
ESCR 10% Igepal® | <= 20 hour | <= 20 hour | F50; ASTM D1963 |
ExxonMobil HDPE HYA 800 High Density Polyethylene Resin Product Description: HYA 800 is a homopolymer HDPE grade, characterized by high stiffness, high rigidity and high flow.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal .. |
|||
ESCR 10% Igepal® | 20 hour | 20 hour | F50; ASTM D1693A |
ExxonMobil LLDPE LL 8446.21 Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 8446 is a linear low density butane copolymer designed to offer excellent processability, whiteness, and fast grinding rate. This UV stabilized resin is ideally suited for ap.. |
|||
ESCR 10% Igepal® | 20 hour @Thickness 2.00 mm, Temperature 40.0 °C |
20 hour @Thickness 0.0787 in, Temperature 104 °F |
0.3 mm notched-plaques; ASTM-D1693 |
Braskem GF4950 HDPE Blow Molding Polyethylene Copolymer HDPE GF4950 is a high-density polyethylene copolymer with well balanced properties between impact and stiffness combined with high environmental stress cracking resistance and processability. It was.. |
|||
ESCR 10% Igepal® | 20 hour | 20 hour | F50; ASTM D1693 |
Carmel Olefins IPETHENE® 4203 Low Density Polyethylene IPETHENE® 4203 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, very good bubble stability in thick-gauge blown film processing, and excellent ESCR. .. |