Material Notes:
Product Description: HYA 600 is a general purpose HDPE resin, characterized by very easy processability, an excellent balance of rigidity and impact strength and a good ESCR.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabilizer: Yes Applications: Drainage PipesFood packagingHousehold and Industrial chemical containers Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D4883
ESCR 100% Igepal® 50 hour
50 hour
F50; ASTM D1963
ESCR 10% Igepal® 20 hour
20 hour
F50; ASTM D1963
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
29 g/10 min

@Load 21.6 kg,
Temperature 190 °C
29 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62

@Time 15.0 sec
62

@Time 0.00417 hour
ASTM D2240
Tensile Stress 13.8 MPa

@Strain 100 %
2000 psi

@Strain 100 %
2 in/min; ASTM D412
Tensile Strength, Yield 26.2 MPa
3800 psi
2 in/min; ASTM D638
Elongation at Break >= 100 %
>= 100 %
2 in/min; ASTM D638
Tensile Modulus 0.965 GPa
140 ksi
2 in/min; ASTM D638
Izod Impact, Notched (ISO) 14.1 kJ/m²
6.70 ft-lb/in²
Area; ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 128 °C
262 °F
ASTM D1525