Material Notes:
Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance. Ideally suited for articles requiring rugged physical performance in cold temperature environments.Availability: Latin America, North America and South America Additive: Anti-gas fading: YesApplications: Automotive ComponentsIndustrial ClosuresRecreation Vehicle – ComponentsWaste CartsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ExxonMobil method
ESCR 10% Igepal® 20 hour
20 hour
F50; ASTM D1963B
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D638
Tensile Strength, Yield 23.4 MPa
3400 psi
ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
2% Secant; ASTM D790B
Flexural Modulus, 1% Secant 1100 MPa
160000 psi
ASTM D790B
Izod Impact, Notched 0.534 J/cm

@Temperature -40.0 °C
1.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point <= 266 °C
<= 511 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C
156 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.2 °C
108 °F
ASTM D648B