Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil LLDPE LL 8446.21 Linear Low Density Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Exxon Chemical
Trade Name LLDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LLDPE LL 8446.21 Linear Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LL 8446 is a linear low density butane copolymer designed to offer excellent processability, whiteness, and fast grinding rate. This UV stabilized resin is ideally suited for applications that require excellent dimensional control and low warpage. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Long Term UV-8 Stabilizer: YesApplications:Consumer ArticlesGeneral Purpose ArticlesTanksToysInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil method
ESCR 100% Igepal® >= 40 hour
>= 40 hour
F50; ASTM D1693A
ESCR 10% Igepal® 20 hour
20 hour
F50; ASTM D1693A
30 hour

@Thickness 1.91 mm
30 hour

@Thickness 0.0750 in
F50; ASTM D1693
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 0.689 GPa
100 ksi
ISO 178
Flexural Modulus, 1% Secant 758 MPa
110000 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point <= 257 °C
<= 495 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 52.2 °C
126 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 36.1 °C
97.0 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved