Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 105 - 180 cm³/g | 105 - 180 cm³/g | Average value: 133 cm³/g Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Viscosity Test | 105 - 158 cm³/g | 105 - 158 cm³/g | Average value: 137 cm³/g Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | DIN-53726 |
Iran Petrochemical (PCC) PVC-S6558 Poly Vinyl Chloride Grade S6558 has low porosity & high bulk density.Applications: pipe and fitting, injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | DIN-53726 |
Iran Petrochemical (PCC) PVC-S7054 Poly Vinyl Chloride Grade S-7054 has high porosity. Therefore it is most suitable for flexible applications. The electrical, mechanical & thermal properties expected of the various applications can be achieved with th.. |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® B 1300 000000 PBT PBT, non-reinforced, injection molding, extrusion |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® B 1305 000000 PBT PBT, non-reinforced, injection molding |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® B 7375 000000 PBT, White Pigment PBT, 25% white pigments, injection molding, improved light reflection, low tendency to warp |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® KU 1-7301 000000 PBT PBT, non-reinforced, injection molding, food contact |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | ISO 307 1157 1628 |
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | Viscosity number |
BASF Ultradur B 4300 G6 BKQ16 15007 PBT |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | Viscosity number |
BASF Ultradur B 4406 G6 BKQ113 7110 30% Glass Filled PBT Ultradur B 4406 G6 BKQ113 7110 is an UL V0 injection molding, pigmented black, PBT grade with 30% glass fiber reinforcement. |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | Viscosity number |
BASF Ultradur B 4406 G6 Q113 30% Glass Filled PBT Ultradur B4406 G6 Q113 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement. |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | Viscosity number; ISO 1628 |
BASF Ultradur S 4090 G4 20% Glass Filled PBT Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio.. |
|||
Viscosity Test | 105 cm³/g | 105 cm³/g | Viscosity number; ISO 1628 |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |