Polymer Property : Viscosity Test = 180 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 105 - 180 cm³/g
105 - 180 cm³/g
Average value: 133 cm³/g Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Viscosity Test 79.0 - 180 cm³/g
79.0 - 180 cm³/g
Average value: 121 cm³/g Grade Count:23
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..