Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : High Load Melt Index = 28 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
High Load Melt Index 28 g/10 min

@Load 21.6 kg,
Temperature 200 °C
28 g/10 min

@Load 47.6 lb,
Temperature 392 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PET 1451
PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14..
High Load Melt Index 28 g/10 min

@Load 21.6 kg
28 g/10 min

@Load 47.6 lb
ISO 1133
Total Finathene® 6002 HDPE, blow molding, pipe  (discontinued **)
FINATHENE® 6002 is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® 6002 has been especially developed for the manufacturing of toys and of b..
High Load Melt Index 28 g/10 min

@Load 21.6 kg
28 g/10 min

@Load 47.6 lb
ISO 1133
Total Lacqtene® 2005 TN 59 HDPE pipe  (discontinued **)
LACQTENE® 2005 TN 59 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2005 TN 59 is best processed between 190 and 230°C.Informa..
High Load Melt Index 28 g/10 min

@Load 21.6 kg,
Temperature 190 °C
28 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Borealis Borstar® BB2581 HDPE for Blow Molding
Borstar BB2581 is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR).Borstar BB2581 is recommended for h..
High Load Melt Index 28 g/10 min

@Load 21.6 kg,
Temperature 190 °C
28 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications
Bormed HE2581-PH is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR). Bormed HE2581-PH can as well be ..