Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Finathene® 6002 HDPE, blow molding, pipe  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® 6002 HDPE, blow molding, pipe  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FINATHENE® 6002 is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® 6002 has been especially developed for the manufacturing of toys and of blow molded bottles for diverse non-aggressive liquids such as food, oil and cosmetics. Its low melt viscosity is particularly suitable for high output processing equipment. Its high rigidity is especially appreciated when bottle weight reduction is critical. FINATHENE® 6002 is best processed at temperatures between 180 and 220°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.959 g/cc
0.0346 lb/in³
ISO 1183
Environmental Stress Crack Resistance 15 hour
15 hour
ASTM D1693-70
Melt Flow 0.30 g/10 min

@Load 2.16 kg
0.30 g/10 min

@Load 4.76 lb
ISO 1133
1.4 g/10 min

@Load 5.00 kg
1.4 g/10 min

@Load 11.0 lb
ASTM D 1238
High Load Melt Index 28 g/10 min

@Load 21.6 kg
28 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.0 MPa
3770 psi
ISO 527
Tensile Strength, Yield 28.0 MPa
4060 psi
ISO 527
Elongation at Break >= 700 %
>= 700 %
ISO 527
Elongation at Yield 8.0 %
8.0 %
ISO 527
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Tensile Impact Strength 80.0 kJ/m²
38.1 ft-lb/in²
Notched, -30°C; ISO 8256
230 kJ/m²
109 ft-lb/in²
Notched, 23°C; ISO 8256
Thermal Properties Metric English Comments
Vicat Softening Point 128 °C
262 °F
ISO 306
Descriptive Properties Value Comments
Food Approval This material complies with the main regulations concerning non-toxicity of plastics materials in contact with food stuffs.
Users viewing this material also viewed the following: