Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 21 g/10 min @Load 21.6 kg, Temperature 300 °C |
21 g/10 min @Load 47.6 lb, Temperature 572 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PPE 1462
(discontinued **) PRE-ELEC PPE 1462 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
High Load Melt Index | 21 g/10 min @Load 21.6 kg, Temperature 190 °C |
21 g/10 min @Load 47.6 lb, Temperature 374 °F |
High Load Melt Index; ASTM D 1238 |
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In.. |
|||
High Load Melt Index | 21 g/10 min @Load 21.6 kg, Temperature 190 °C |
21 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Formosa Plastics Formolene® HL3721 Sheet and Thermoforming HDPE
(discontinued **) Medium Density Hexene CopolymerApplications: Geomembranes, gas and chemical tank containment liners, landfill liners.Formolene HL3721 is tailored for extrusion applications requiring good processabi.. |
|||
High Load Melt Index | 21 g/10 min @Load 21.6 kg, Temperature 190 °C |
21 g/10 min @Load 47.6 lb, Temperature 374 °F |
Condition F; ASTM D1238 |
Formosa Plastics Formolene® HP5221 Pipe HDPE
(discontinued **) High Density Hexene Copolymer Formolene® HP5221 is a high performance copolymer that is designed for the most demanding requirements of corrugated pipe applications. Formolene® HP5221 meets the re.. |
|||
High Load Melt Index | 21 g/10 min @Load 21.6 kg, Temperature 190 °C |
21 g/10 min @Load 47.6 lb, Temperature 374 °F |
Condition F; ASTM D1238 |
Formosa Plastics Formolene® E602 Pipe HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin for Non-Pressure Pipe Extrusion Applications Formolene® E602 is a high performance copolymer that is designed for the most demanding r.. |
|||
High Load Melt Index | 21 g/10 min @Load 21.6 kg, Temperature 190 °C |
21 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: geomembrane, gas and chemical containment liners, landfill linersInfor.. |
|||
High Load Melt Index | 21 g/10 min @Load 21.6 kg, Temperature 190 °C |
21 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® K307 MDPE Hexene Copolymer Extrusion grade hexene copolymerCharacteristics: good processability, excellent melt strength, broad fusion range, outstanding stress crack resistance, meets the requirements of GRI-GM13. Meets A.. |
|||
High Load Melt Index | 21 g/10 min @Load 21.6 kg, Temperature 190 °C |
21 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow DGDA-2475 NT High Density Polyethylene Resin DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in corrugated pipe applications. It has been specifically designed for extrusion of corrugated pipes with the.. |