Material Notes:
High Density Polyethylene High Molecular Weight Bi-Modal Resin for Non-Pressure Pipe Extrusion Applications Formolene® E602 is a high performance copolymer that is designed for the most demanding requirements of corrugated pipe applications. Formolene® E602 meets the requirements of the PPI third party certification program for use in AASHTO M294 corrugated pipe. Formolene® E602 has a cell class of 436460/446460 per ASTM D3350-05Applications: Highway Drainage Pipe, Agricultural Drainage Pipe and Storm Water Drainage PipePhysical properties reported herein were determined on compression molded specimens prepared in accordance with Procedure C of ASTM D1928.Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 24 hour
>= 24 hour
ESCR by NCLS; ASTM F2136
ESCR 100% Igepal® >= 150 hour
>= 150 hour
Condition B, F<sub>50</sub>; ASTM D1693
Melt Flow 0.15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
High Load Melt Index 21 g/10 min

@Load 21.6 kg,
Temperature 190 °C
21 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Condition F; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.9 MPa
3900 psi
2" (50mm) per min, Type IV; ASTM D638
Elongation at Break >= 600 %
>= 600 %
2" (50mm) per min, Type IV; ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -90.0 °C
<= -130 °F
ASTM D746