Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1800 - 3600 cP | 1800 - 3600 cP | Spindle # 4, rpm 60 |
Michelman® SofTak® 1637 Non-skid coating Description: Non-skid coating.Usage: SofTak® 1637 is a gluable nonskid coating with the added benefit of good scuff and water resistance, oil resistance and a "leather-like" feel. This product is.. |
|||
Brookfield Viscosity | >= 1800 cP | >= 1800 cP | 0.3% sol. - 22° HT, Brookfield LV 3 rpm spindle n°2 – after 24 h; TI-2102 |
Solvay RHODOPOL® 50 MD Surfactant Description: Rhodopol® 50 MD is Xanthan Gum that turns into viscous colloidal solution on dispersion in water. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing a.. |
|||
Brookfield Viscosity | 1800 - 3000 cP | 1800 - 3000 cP | RVF #4 sp @ 20 rpm @ 27°C |
3M Scotch-Weld™ Hi-Strength Postforming 4693H High Performance Industrial Plastic Adhesives Features: High Viscosity grade in collapsible tubes for flow applicationsClear elastomeric adhesives with high immediate bond strength, long tack range and contact bond propertiesExhibits outstandin.. |
|||
Brookfield Viscosity | 1800 - 2000 cP | 1800 - 2000 cP | 1.5 min mixed |
BCC Products BC 8870 Polyurethane Elastomer BC8870 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig.. |
|||
Brookfield Viscosity | 1800 - 3300 cP | 1800 - 3300 cP | RVT #2 spindle @ 20 rpm |
3M Scotch-Weld™ RT38 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |