Solvay RHODOPOL® 50 MD Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODOPOL® 50 MD Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rhodopol® 50 MD is Xanthan Gum that turns into viscous colloidal solution on dispersion in water. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent.Identification: XANTHAN GUMCAS: 11138 – 66 – 2Available in: Asia Pacific, Europe, Latin America and North America.Applications: Painting, Public works, Pottery industry and Industrial and household cleanersInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Particle Size >= 300 µm
>= 300 µm
<2%, 50 Mesh; TI-2087
pH 5.0 - 7.5
5.0 - 7.5
1% aq. Sol.; TI-2076
Brookfield Viscosity >= 1800 cP
>= 1800 cP
0.3% sol. - 22° HT, Brookfield LV 3 rpm spindle n°2 – after 24 h; TI-2102
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Cream Powder
Loss on drying <13%
TI-0515