Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1800 - 3600 cP | 1800 - 3600 cP | Spindle # 4, rpm 60 |
Michelman® SofTak® 1637 Non-skid coating Description: Non-skid coating.Usage: SofTak® 1637 is a gluable nonskid coating with the added benefit of good scuff and water resistance, oil resistance and a "leather-like" feel. This product is.. |