Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 25 hour | 25 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 59A HDPE Injection Molding Resin Features: Homopolymer, high drop impact resistance and high stiffness.Applications: Juice, water containers, personal protective equipment, grain elevator buckets, designed for accumulator and recip.. |
|||
Environmental Stress Crack Resistance | >= 25 hour | >= 25 hour | |
Kazanorgsintez 276-288 High Density Polyethylene Composite Production Method: Compositions are achieved by gaseous-phase method. Application: Composition is intended for production of polymer film fibers contacting bulk food.Information Provided by Kaza.. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LB5604 High Density Polyethylene ApplicationsThe PETROTHENE LB 5604 series of polyethylene resins exhibits good stiffness and environmental stress cracking resistance. Typical applications include household chemical and person car.. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LR734011 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LR734045 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | |
JPJ Technologies 5200B HDPE Blow Molding Information provided by JPJ Technologies |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F50; ASTM D1693 |
CPC - Vycom SEABOARD™ GRIP-X™ Slip Resistant High Density Polyethylene (HDPE) Grip-X is a UV stabilized high density polyethylene (HDPE) sheet formulated to meet demanding conditions of the marine industry. Grip-X is manufactured with a special surface treatment and stipulate.. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F50; ASTM D1693 |
CPC - Vycom SEABOARD™ LITE High density polyethylene (HDPE) Seaboard Lite is a high density polyethylene (HDPE) sheet formulated to meet the specific requirements of marine and other outdoor environments. Seaboard Lite is UV stable and will withstand the ele.. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F50; ASTM D1693 |
CPC - Vycom SEABOARD™ Premier High density polyethylene (HDPE) Seaboard High Density Polyethylene (HDPE) is the toughest marine grade polymer sheet available. This UV stable product has scratch resistance, excellent impact, and stiffness, yet it is easy to mach.. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F50; ASTM D1693 |
CPC - Vycom SEABOARD™ Supreme DS High density polyethylene (HDPE) Seaboard DS is a high density polyethylene (HDPE) foam core product with a specially formulated skin to add stiffness and Dimensional Stability. This new product from Compression Polymers combines l.. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F50, 100% Igepal, Bent strip test, slit; ASTM D-1693 |
Bapolene® 2272 Polyethylene, Injection Grade Bapolene LL2272 is a high flow, narrow molecular weight distribution, linear low density polyethylene injection resin. This resin offers excellent stress cracking resistance, flex life, low tempera.. |
|||
Environmental Stress Crack Resistance | 25 hour | 25 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Novapol® HB-L455-A HDPE Blow Molding Resin
(discontinued **) Molded Plaque Properties. Features: excellent processability on high speed, multiple-head blow molding lines, good balance of physical and molding properties.Applications: chemical bottles, toys.Da.. |