Bapolene® 2272 Polyethylene, Injection Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 2272 Polyethylene, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene LL2272 is a high flow, narrow molecular weight distribution, linear low density polyethylene injection resin. This resin offers excellent stress cracking resistance, flex life, low temperature toughness and low warpage. This product meets FDA standards for food contact applications.Applications: Industrial containers, housewares, caps and closures, and color concentrates.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 25 hour
25 hour
F50, 100% Igepal, Bent strip test, slit; ASTM D-1693
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.1 MPa
1750 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 280 %
280 %
2 in/min (50 mm/min); ASTM D638
Modulus of Elasticity 0.324 GPa
47.0 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D-746
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution