ExxonMobil Escorene® LD-400 LDPE Medium/High Voltage Insulation  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Wire/Cable Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® LD-400 LDPE Medium/High Voltage Insulation  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer resin designed for electrical applications.Applications: Base resin for medium voltage power cable insulation compounds.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
Exxon Method
Environmental Stress Crack Resistance <= 1.0 hour
<= 1.0 hour
F50, Condition A; ASTM D-1693
Melt Flow 2.8 g/10 min
2.8 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ASTM D2240
Tensile Strength, Ultimate 9.60 MPa
1390 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 0.186 GPa
27.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 108 °C
226 °F
Exxon Method
Brittleness Temperature <= -72.0 °C
<= -97.6 °F
ASTM D746
Electrical Properties Metric English Comments
Dielectric Constant 2.25

@Frequency 1e+6 Hz
2.25

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.4 kV/mm

@Thickness 3.17 mm
518 kV/in

@Thickness 0.125 in
ASTM D149
Dissipation Factor 0.00010

@Frequency 1e+6 Hz
0.00010

@Frequency 1e+6 Hz
ASTM D150