Material Notes:
Molded Plaque Properties. Features: high flow.Applications: general purpose, housewares.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
ASTM D792
Environmental Stress Crack Resistance 1.0 hour
1.0 hour
F50, Condition A, ASTM D1693, 100% Igepal
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.0 MPa
1890 psi
ASTM D638
Elongation at Break 190 %
190 %
ASTM D638
Flexural Modulus 0.390 GPa
56.6 ksi
ASTM D790
Processing Properties Metric English Comments
Melt Temperature 160 - 230 °C
320 - 446 °F
Copyright © lookpolymers.com All Rights Reserved