Physical Properties Metric English Comments
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 230 °C
50 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Premix Thermoplastics PRE-ELEC® PP 1383
PRE-ELEC PP 1383 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Melt Flow 50 g/10 min

@Load 10.0 kg,
Temperature 260 °C
50 g/10 min

@Load 22.0 lb,
Temperature 500 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East)
XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Melt Flow 50 g/10 min

@Load 21.6 kg,
Temperature 200 °C
50 g/10 min

@Load 47.6 lb,
Temperature 392 °F
ASTM D1238
I. Stern 750SW Medium Impact Natural ABS
Features:Easy color-abilityInjection MoldingApplicationsOffice equipmentElectronic partsSpools, ReelsInformation provided by I. Stern & Co. Inc.
Melt Flow 50 g/10 min

@Load 10.0 kg,
Temperature 220 °C
50 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Kingfa HF-626 Flame Retardant ABS
Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowHigh impact resistanceApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 265 °C
50 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East)
VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils.
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 266 °C
50 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East)
VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils.
Melt Flow 50 g/10 min

@Load 10.0 kg,
Temperature 300 °C
50 g/10 min

@Load 22.0 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics LNP Stat-kon DX07323 PC+ABS
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 265 °C
50 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 265 °C
50 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East)
Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 266 °C
50 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East)
Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 265 °C
50 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East)
VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage.
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 266 °C
50 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East)
VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage.
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 230 °C
50 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Borealis Daplen™ SB4411/2 Polypropylene Compound Elastomer and Mineral Modified
Daplen SB4411/2 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. The product is available in black, but other colors can be provided on request.Daplen ..
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 260 °C
50 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C6303 PC+ABS
LNP* Lubricomp* Cycoloy_C6303 compound is a Wear resistant (5% PTFE), flame retardant PC+ABS. High heat and good hydrolytic stability. UL listing from Japan and Pacific.
Copyright © lookpolymers.com All Rights Reserved