I. Stern 750SW Medium Impact Natural ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer I. Stern & Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF I. Stern 750SW Medium Impact Natural ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Easy color-abilityInjection MoldingApplicationsOffice equipmentElectronic partsSpools, ReelsInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 4.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
35 g/10 min

@Load 10.0 kg,
Temperature 220 °C
35 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
50 g/10 min

@Load 21.6 kg,
Temperature 200 °C
50 g/10 min

@Load 47.6 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength 47.97 MPa
6958 psi
ASTM D638
Elongation at Yield 15 %
15 %
ASTM D638
Flexural Strength 68.5 MPa
9940 psi
ASTM D790
Flexural Modulus 2.350 GPa
340.8 ksi
ASTM D790
Izod Impact, Notched 2.46 J/cm
4.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Heat Distortion Temperature 85.0 °C
185 °F
ASTM D648