Physical Properties Metric English Comments
Melt Flow 5.3 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.3 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D 1238
SABIC Innovative Plastics Cycolac® FR30U ABS
Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 5.3 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.3 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific)
Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Hytrel® 4053FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..