Physical Properties Metric English Comments
Melt Flow 1.6 g/10 min

@Load 5.00 kg
1.6 g/10 min

@Load 11.0 lb
ASTM D 1238
Total Finathene® 7208 HDPE extrusion resin  (discontinued **)
Applications: monofilament, slit tape, woven and knitted fabrics, specialty filmsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics ..
Melt Flow 1.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan..
Melt Flow 1.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th..
Melt Flow 1.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas..
Melt Flow 1.6 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.6 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) EX 1 HF 7740F2 High Density Polyethylene
EX1 (HF 7740F2) is high density polyethylene with Butene-1 as co monomer. It is a medium molecular mass with a narrow molar mass distribution.Application: stretched film tape used in manufacture o..
Melt Flow 1.6 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.6 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ISO 1133
Styron EMERGEâ„¢ 5302 Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ ABS 5302 is a black, 20% glass-filled ABS which is suitable for use in a wide variety of internal structural component applications in the information technology market. Applications: ..