Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Unipetrol PE HD LITEN® PL 10 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Unipetrol RPA
Trade Name PE HD LITEN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unipetrol PE HD LITEN® PL 10 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pipe applications.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ISO 1183
ESCR 100% Igepal® >= 1000 hour

@Temperature 50.0 °C
>= 1000 hour

@Temperature 122 °F
ASTM D1693
Carbon Black Loading 2.4 %
2.4 %
ISO 6469
Melt Flow 0.080 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.080 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
0.45 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ISO 868
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO 527
Elongation at Yield 9.0 %
9.0 %
ISO 527
Flexural Modulus 0.800 GPa
116 ksi
ISO 178
Charpy Impact, Notched 0.120 J/cm²

@Temperature 23.0 °C
0.571 ft-lb/in²

@Temperature 73.4 °F
ISO 179
0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 119 °C
246 °F
ISO 306
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved