Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.0931 g/m²/day @Temperature 38.0 °C |
0.00600 g/100 in²/day @Temperature 100 °F |
90% RH; ExxonMobil Method |
ExxonMobil Metallyte™ 12MM281 OPP Film Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. 12MM281 is designed for use as the center web of a triplex adhesive lamination. The treated s.. |
|||
Water Vapor Transmission | 0.0931 g/m²/day @Temperature 38.0 °C |
0.00600 g/100 in²/day @Temperature 100 °F |
90% RH; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM882 OPP Film Product Description: An ultra high barrier (UHB), biaxially oriented, multilayer polypropylene film. In addition to an excellent water vapor barrier, this film has an exceptional barrier to oxygen, .. |
|||
Water Vapor Transmission | 0.0931 g/m²/day @Temperature 38.0 °C |
0.00600 g/100 in²/day @Temperature 100 °F |
90% RH; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM883 OPP Film Product Description: An ultra high barrier (UHB), biaxially oriented multilayer polypropylene film. This film has an exceptional barrier to oxygen, flavors and aromas and has an excellent water vapo.. |