Material Notes:
Product Description: An ultra high barrier (UHB), biaxially oriented, multilayer polypropylene film. In addition to an excellent water vapor barrier, this film has an exceptional barrier to oxygen, flavors and aromas. The non-metalized PE compatible layer is designed for excellent adhesion of polyethylene for extrusion coating or extrusion laminations. This layer will lap seal to a range of polyethylene films. This film has excellent and consistent flip characteristics and an be treated for printing and adhesive laminating.Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, North America and South AmericaKey Features:Outstanding oxygen barrier Outstanding moisture and light barriersOutstanding aroma and flavor barrierEasily converted on the meal sideExcellent puncture resistanceLap sealable to PEStable CoF on unmetallized surfaceFeatures:Flavor & Aroma BarrierGas BarrierGrease ResistantLap Sealable to PELight BarrierMoisture BarrierOxygen BarrierPuncture ResistantTwo Side ProcessableApplications:Biscuits/Cookie/CrackersConfectionery, Chocolate Crisps and SnacksDry Foods and Beverage PowdersHealth and Beauty CareHousehold and DetergentsPet Food Uses: HFFS Flexible PackagingLidding – Flexible PackagingPouches – Flexible PackagingPre-made Bags – Flexible PackagingVFFS Flexible PackagingProcessing Method: Extrusion Coating, Middle Web Extrusion Lamination and Outer Web Adhesive LaminationInformation provided by ExxonMobil
Physical Properties Metric English Comments
Water Vapor Transmission 0.0931 g/m²/day

@Temperature 38.0 °C
0.00600 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
Oxygen Transmission Rate 0.101 cc/m²/day

@Temperature 23.0 °C
0.00650 cc/100 in²/day

@Temperature 73.4 °F
ExxonMobil Method
Thickness 18.0 microns
0.710 mil
ExxonMobil Method
Coating Weight 16.2 g/m²
10.1 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 124 MPa
18000 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 234 MPa
34000 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 4.5 %

@Temperature 135 °C,
Time 432 sec
4.5 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Shrinkage, TD 4.5 %

@Temperature 135 °C,
Time 432 sec
4.5 %

@Temperature 275 °F,
Time 0.120 hour
ExxonMobil Method
Optical Properties Metric English Comments
Optical Density 2.8
2.8
ExxonMobil Method
Transmission, Visible 0.20 %
0.20 %
ExxonMobil Method
Descriptive Properties Value Comments
Yield 42900 in2/lb