Physical Properties Metric English Comments
Thickness 94.0 microns
3.70 mil
Typical; ASTM D374
DuPont™ Nomex® 414 Paper, 3.4 mil Nominal Thickness
Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand..
Thickness 94.0 microns
3.70 mil
Liner
3M 7840TL Laser Toner Printable Polyester Label Material
3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi..
Thickness 94.0 microns
3.70 mil
Liner
3M 7850TL Laser Toner Printable Polyester Label Material
3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for..
Thickness 94.0 microns
3.70 mil
Liner
3M FM016 Indoor UL Recognized Clear Polyester Overlaminate Label Product
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
Thickness 94.0 - 106 microns
3.70 - 4.17 mil
ASTM D374
CEN® Electronic Material CV Polyimide Film, 4 Mil Thickness
CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup..
Thickness 94.0 microns
3.70 mil
Total; ASTM D3752
3M 5480 PTFE Skived Film Tape
3M™ PTFE Skived Film Tape 5480 is a film backing with a silicone adhesive.Information provided by 3M
Thickness 94.0 microns
3.70 mil
Total; ASTM D3752
3M 5490 PTFE Extruded Film Tape
3M™ PTFE Extruded Film Tape has a film backing with a silicone adhesive.Information provided by 3M
Thickness 94.0 microns
3.70 mil
3M 8507 Repulpable Forms-Splicing Tape
3M™ Repulpable Forms-Splicing Tape 8507 is a specially engineered tape for forms-splicing with a thin, semi-bleached backing, a heat resistant adhesive and skip-slit for easy separation; all comple..
Thickness 94.0 microns
3.70 mil
3M 910 Repulpable Forms-Splicing Tape
3M™ Repulpable Forms-Splicing Tape 910 is a single-coated repulpable construction using a release coated, semi-bleached kraft paper backing and a blue, high performance adhesive.Information provide..
Thickness 94.0 microns
3.70 mil
3M 914 Repulpable Forms-Splicing Tape
3M™ Repulpable Forms-Splicing Tape 914 is a specially engineered forms-splicing tape using a thing, release-coated semi-bleached kraft paper backing and a blue, high performance repulpable adhesive..
Thickness 94.0 microns
3.70 mil
Faceside Adhesive
3M 93020LE High Strength Double Coated Tape with Adhesive 300LSE
3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl..
Thickness 94.0 microns
3.70 mil
Backside Adhesive
3M 93020LE High Strength Double Coated Tape with Adhesive 300LSE
3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl..
Thickness 94.0 microns
3.70 mil
Facestock
3M 7884 White Vinyl Label Material
Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and..
Thickness 94.0 - 106 microns
3.70 - 4.17 mil
CEN® Electronic Material CN Polyimide Film, 4 Mil Thickness
CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca..