3M 8507 Repulpable Forms-Splicing Tape

Category Polymer , Tape
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 8507 Repulpable Forms-Splicing Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Repulpable Forms-Splicing Tape 8507 is a specially engineered tape for forms-splicing with a thin, semi-bleached backing, a heat resistant adhesive and skip-slit for easy separation; all completely repulpable so scrap is never contaminate.Information provided by 3M
Physical Properties Metric English Comments
Thickness 94.0 microns
3.70 mil
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 73.7 MPa
10700 psi
Film Tensile Strength at Break, TD 41.1 MPa
5960 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Descriptive Properties Value Comments
Adhesive Type Blue, repulpable
Appearance Off-white