Physical Properties Metric English Comments
Thickness 70.0 microns
2.76 mil
P & P Technology Oriented Wires In Silicone
P & P Technology SP, SS, SR, SW & SF Ranges of gasket materials consist of Monel or aluminum wires embedded into solid silicone, sponge silicone or fluorosilicone, a fire retardant variant is also a..
Thickness 70.0 - 127 microns
2.76 - 5.00 mil
Average value: 82.4 microns Grade Count:7
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Thickness 70.0 - 3180 microns
2.76 - 125 mil
Average value: 821 microns Grade Count:17
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Thickness 70.0 microns
2.76 mil
Isoflon Tisoflon® 3G Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Thickness 70.0 microns
2.76 mil
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.
Thickness 70.0 microns
2.76 mil
Borealis Borstar® FB4250T LLDPE for Blown Film
Borstar FB4250 is well suited for a wide range of film applications due to its properties. The well balanced mechanical properties will improve the functionality of the films or allow for material ..
Thickness 70.0 microns
2.76 mil
Film
Topas Advanced Polymers TOPAS® 5013F-04 Cyclic Olefin Copolymer (COC)
TOPAS® 5013F-04 is a high temperature film extrusion grade for blends. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity ..
Thickness 70.0 microns
2.76 mil
Film
Topas Advanced Polymers TOPAS® 6013F-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6013F-04 is a high temperature, general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and p..
Thickness 70.0 microns
2.76 mil
Film
Topas Advanced Polymers TOPAS® 8007F-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007F-04 is a general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and..
Thickness 70.0 microns
2.76 mil
Film
Topas Advanced Polymers TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC)
TOPAS® 9506F-500 is a high clarity extrusion grade for use in shrink, food and medical packaging as either a discrete layer in multilayer film or in blends with polyethylene. It is designed to del..
Thickness 70.0 microns
2.76 mil
Film
Topas Advanced Polymers TOPAS® 8007F-400 Cyclic Olefin Copolymer (COC)
TOPAS® 8007F-400 is a robust film extrusion grade designed for blending with polyethylene (PE). It is a moderate clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, ..
Thickness 70.0 - 80.0 microns
2.76 - 3.15 mil
CEN® Electronic Material CN Polyimide Film, 3 Mil Thickness
CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca..
Thickness 70.0 - 80.0 microns
2.76 - 3.15 mil
ASTM D374
CEN® Electronic Material CV Polyimide Film, 3 Mil Thickness
CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup..