Physical Properties Metric English Comments
Thickness 12.7 - 127 microns
0.500 - 5.00 mil
Recommended range for processing
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin
FPs016-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
Thickness 70.0 - 127 microns
2.76 - 5.00 mil
Average value: 82.4 microns Grade Count:7
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Thickness 76.2 - 127 microns
3.00 - 5.00 mil
per coat; minimum three coats recommended
Industrial Nanotech Nansulateâ„¢ GP Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general purpose insulation.NANSULATEâ„¢ liquid applied insulation is a prem..
Thickness 76.2 - 127 microns
3.00 - 5.00 mil
per coat; minimum three coats recommended
Industrial Nanotech Nansulateâ„¢ High Heat Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology.NANSULATEâ„¢ liquid applied insulation is a premium industrial grade rust proofing protective ..
Thickness 76.2 - 127 microns
3.00 - 5.00 mil
per coat; minimum three coats recommended
Industrial Nanotech Nansulateâ„¢ PT Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general insulation use for pipes, tanks, and metallic surfaces.NANSULATEâ„¢..
Thickness 100 - 127 microns
3.94 - 5.00 mil
Available Range
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Thickness 102 - 127 microns
4.00 - 5.00 mil
Side 2
Arlon 70011B016 0.016" (0.406 mm) Uncured Silicone Rubber with Prime Coated Polyester Fabric Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Controltac™ 160 Graphic Film
4-mil, opaque white, opaque black and translucent white vinyl film with a matte finish; Pressure-activated adhesives for easy sliding, tacking, snap up and repositioning; Film series 160C-10 also ha..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Controltac™ 3545C Removable Graphic Film with Comply™ Adhesive
4-mil white, opaque, polyolefin film; Chloride-free film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast and easy application; Remova..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Controltac™ 8640C ES Graphic Film with Comply™ Adhesive
This 4-mil film offers great versatility along with slidable, repositionable, pressure activated adhesive. This long term durable and removable film has excellent hiding power and stability, making ..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Controltac™ 8655C ES Changeable Graphic Film with Comply™ Adhesive
3M™ Controlact™ Plus Changeable Graphic Film with Comply™ Adhesive 8655C ES combines the features found in Controltac and Comply adhesive technologies, including pressure activation, positionabil..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Controltac™ IJ160C Graphic Film with Comply™ Adhesive
4-mil, opaque white, vinyl film with a matte finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Film IJ160C-10 also has Comply™ Adhesive air release channels ..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Scotchcal™ 3470 Graphic Film
4-mil, opaque white and opaque black, vinyl film with a matte finish; Pressure-sensitive adhesive; Excellent hiding power; Removable with heatInformation provided by 3M
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Scotchcal™ IJ355%-10 Changeable Graphic Film
4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-sensitive adhesive; Changeable for clean removable without heat or chemicalsInformation provided by 3M
Thickness 76.2 - 127 microns
3.00 - 5.00 mil
Overall
Arlon R33670N004 0.004" (0.102 mm) Uncured Silicone Rubber with K2030 PEN Film Substrate
Design/Construction:Side 1: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Inf..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Controltac™ 160C Graphic Film with Comply™ Adhesive
4-mil, opaque white, opaque black and translucent white vinyl film with a matte finish; Pressure-activated adhesives for easy sliding, tacking, snap up and repositioning; Film series 160C-10 also ha..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Controltac™ 162-10 Graphic Film
4-mil, opaque white, or clear vinyl film; Slideable and repositionable; Excellent hiding power (white film); Easily removable and Outstanding resistance to dirt and other environmental factors and w..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Controltac™ 162-114 Graphic Film
4-mil, opaque white, or clear vinyl film; Slideable and repositionable; Excellent hiding power (white film); Easily removable and Outstanding resistance to dirt and other environmental factors and w..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Controltac™ 3500C Changeable Graphic Film with Comply™ Adhesive
4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast, easy, bub..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Controltac™ IJ160 Graphic Film
4-mil, opaque white, vinyl film with a matte finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Film IJ160C-10 also has Comply™ Adhesive air release channels ..
Thickness 114 - 127 microns
4.50 - 5.00 mil
with adhesive
3M Scotchcal™ 3475 Graphic Film
4-mil, opaque white and opaque black, vinyl film with a matte finish; Pressure-sensitive adhesive; Excellent hiding power; Removable with heatInformation provided by 3M