Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 216 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 140 - 216 microns
5.50 - 8.50 mil
Side 2
Arlon 19566R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The..
Thickness 140 - 216 microns
5.50 - 8.50 mil
Side 2
Arlon 19576R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat..
Thickness 140 - 216 microns
5.50 - 8.50 mil
Side 2
Arlon R34896R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of..
Thickness 165 - 216 microns
6.50 - 8.50 mil
Overall
Arlon 47561R007 0.0075" (0.190 mm) Uncured Rubber
Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not ..
Thickness 165 - 216 microns
6.50 - 8.50 mil
Overall
Arlon 47576R007 0.0075" (0.190 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mate..
Thickness 140 - 216 microns
5.50 - 8.50 mil
Side 1
Arlon 51970R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, or ..
Thickness 165 - 216 microns
6.50 - 8.50 mil
Overall
Arlon 47573R007 0.0075" (0.190 mm) Cured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured RubberSide 2: Cured Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifica..
Copyright © lookpolymers.com All Rights Reserved