Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 165 microns | 6.50 mil | Total |
Parker Chomerics CHO-FAB CFT Shielding Tape Conductive Adhesive Nickel-Plated FabricDescription: CHO-FAB® tape is a corrosion resistant nickel-plated cloth coated with Chomerics’ highly conductive pressure-sensitive adhesive. CHO-FAB® tape.. |
|||
Thickness | 165 microns | 6.50 mil | |
Hexcel® HexForce™ 130 Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |
|||
Thickness | >= 165 microns | >= 6.50 mil | Side 2 |
Arlon 49581R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The.. |
|||
Thickness | 165 microns | 6.50 mil | Side 1 |
Arlon 55191R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Thickness | 165 microns | 6.50 mil | Side 2 |
Arlon 55191R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Thickness | 165 microns | 6.50 mil | Total (excluding liner) |
3M 9741R Double Coated Tape 3M™ Double Coated Tape 9741 is a 6.5 mil double coated tape utilizing a 0.5 mil hand-tearable polyester film heavily coated on both sides with 3 mils of an ultra high peel acrylic adhesive system. .. |
|||
Thickness | 165 microns | 6.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55586XC028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 165 microns | 6.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55866R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Thickness | 165 microns | 6.50 mil | side 2; Arlon SQA-TMS-003 |
Arlon 55946C028 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 165 microns | 6.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber This data represents typical values for the production mate.. |
|||
Thickness | 165 microns | 6.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55986C028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: N/ASide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: LDPEThis data represents typical values for the pro.. |
|||
Thickness | 165 microns | 6.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55986R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material.. |
|||
Thickness | 165 microns | 6.50 mil | ASTM D3652 |
3M 3903 Vinyl Duct Tape 3M™ Vinyl Duct Tape 3903 is a general purpose duct tape with a rubber adhesive and hand tearable, embossed vinyl backing.Information provided by 3M |
|||
Thickness | 165 microns | 6.50 mil | Total; ASTM D3652 |
3M 4201 Lead Foil Tape Permanent acrylic adhesiveInformation provided by 3M |
|||
Thickness | 165 - 216 microns | 6.50 - 8.50 mil | Overall |
Arlon 47561R007 0.0075" (0.190 mm) Uncured Rubber Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not .. |
|||
Thickness | 165 - 216 microns | 6.50 - 8.50 mil | Overall |
Arlon 47576R007 0.0075" (0.190 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mate.. |
|||
Thickness | 165 microns | 6.50 mil | side 2; Arlon SQA-TMS-003 |
Arlon 55096R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: uncured silicone rubber |
|||
Thickness | 165 microns | 6.50 mil | side 2; Arlon SQA-TMS-003 |
Arlon 55106R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Thickness | 165 microns | 6.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55106R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silic.. |
|||
Thickness | 165 microns | 6.50 mil | side 2; Arlon SQA-TMS-003 |
Arlon 55146R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Thickness | 165 microns | 6.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55146XA028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data represents typical values for the production mat.. |
|||
Thickness | 165 microns | 6.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55276B028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data represents typical values for the production mate.. |
|||
Thickness | 165 microns | 6.50 mil | Layer 1; Arlon SQA-TMS-003 |
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Thickness | >= 165 microns | >= 6.50 mil | Side 1 |
Arlon R31551R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | >= 165 microns | >= 6.50 mil | Side 2 |
Arlon R31551R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 165 - 203 microns | 6.50 - 8.00 mil | Overall |
Arlon 45561R007 0.007"(0.178 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not .. |
|||
Thickness | 165 - 216 microns | 6.50 - 8.50 mil | Overall |
Arlon 47573R007 0.0075" (0.190 mm) Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured RubberSide 2: Cured Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifica.. |
|||
Thickness | 165 microns | 6.50 mil | side 2; Arlon SQA-TMS-003 |
Arlon 55276R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Thickness | 165 microns | 6.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55276R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silic.. |
|||
Thickness | 165 microns | 6.50 mil | Layer 1; Arlon SQA-TMS-003 |
Arlon 55279R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |