Physical Properties Metric English Comments
Thickness 330 microns
13.0 mil
Polystrand ThermoPro™ IE6010 Unitape Unidirectional Polypropylene-Glass Composite
Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer ..
Thickness 330 microns
13.0 mil
Polystrand ThermoPro™ IE6021 ECR Unitape Unidirectional Polyethylene-Glass Composite
Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer ..
Thickness 330 microns
13.0 mil
Total; ASTM D374
Parker Chomerics T-Wings Heat Spreaders
Description: Chomerics’ family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are inappropriate. T-Wing spreade..
Thickness 330 microns
13.0 mil
Parker Chomerics T-Wing™ Heat Spreader
Chomerics family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are not appropriate. T-Wing spreaders consist of..
Thickness 330 microns
13.0 mil
Polystrand ThermoBallistic™ TBS8010X X-Ply Cross-Ply Polypropylene-Glass Composite
2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoBallistic laminates combine continuous S-Glass (ThermoBallistic-S™) structural fibers with a proprietary polypropylene thermoplastic poly..
Thickness 330 microns
13.0 mil
Hexcel® HexForce™ 2523 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 330 microns
13.0 mil
Hexcel® HexForce™ 383 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
Thickness 330 microns
13.0 mil
Nominal
DuPont™ Nomex® 419 Paper, 13 mil Nominal Thickness
Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: ..
Thickness 330 microns
13.0 mil
Substrate; Arlon SQA-TMS-003
Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: PolyethyleneLayer 1: Cured Silicone RubberLayer 2: Uncured Silicone RubberSubstrate: 11523 Style FiberglassThis data represents typical values for the production mate..
Thickness 330 - 432 microns
13.0 - 17.0 mil
Overall
Arlon 28941C015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place ..
Thickness 330 - 432 microns
13.0 - 17.0 mil
Overall
Arlon 31570R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a HDPE Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat..
Thickness 330 - 432 microns
13.0 - 17.0 mil
Side 1
Arlon 31570R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a HDPE Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat..
Thickness 330 microns
13.0 mil
Overall; Arlon SQA-TMS-003
Arlon 51112R013 0.013" (0.330 mm) Cured, Self Fusing, Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured, Self Fusing, Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material. The data sho..
Thickness 330 microns
13.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 55173R045 0.045" (1.14 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Product Use: Press PadAppearance: Red silicone rubber on f..
Thickness 330 microns
13.0 mil
Side 2; Arlon SQA-TMS-003
Arlon 55173R045 0.045" (1.14 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Product Use: Press PadAppearance: Red silicone rubber on f..
Thickness 330 microns
13.0 mil
7500 Fiberglass, Substrate
Arlon 75400R045 0.045" (1.14 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info..
Thickness >= 330 microns
>= 13.0 mil
Side 1
Arlon R33920W028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: White gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, ..
Thickness 330 microns
13.0 mil
3M Nextel™ AF-12 Aerospace Woven Fabric 312
Information provided by 3M
Thickness >= 330 microns
>= 13.0 mil
Side 2
Arlon 51576R027 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat..
Thickness 330 - 381 microns
13.0 - 15.0 mil
Overall
Arlon R31651R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
Thickness 330 microns
13.0 mil
Overall; Arlon SQA-TMS-003
Arlon R35798R013 0.013" (0.330 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 Fiberglass Side 2: Uncured Silicone RubberThis data represents typic..
Thickness 330 microns
13.0 mil
3M Nextel™ AF-12 Industrial Woven Fabric 312
Information provided by 3M
Thickness 330 microns
13.0 mil
3M Nextel™ XN-513 Woven Fabric 720
Information provided by 3M