Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 330 - 432 microns | 13.0 - 17.0 mil | Overall |
Arlon 28941C015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 330 - 432 microns | 13.0 - 17.0 mil | Overall |
Arlon 31570R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a HDPE Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat.. |
|||
Thickness | 330 - 432 microns | 13.0 - 17.0 mil | Side 1 |
Arlon 31570R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a HDPE Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat.. |