Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 229 - 381 microns
9.00 - 15.0 mil
Total Construction
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam
Information provided by Rogers Corporation.
Thickness 320 - 380 microns
12.6 - 15.0 mil
Beijing Evergrow Resources ASHRAE HEPA-W29 Glass Fiber Paper
Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applicat..
Thickness 320 - 380 microns
12.6 - 15.0 mil
Beijing Evergrow Resources ASHRAE HEPA-W85 Glass Fiber Paper
Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applicat..
Thickness 229 - 381 microns
9.00 - 15.0 mil
Overall
Arlon 912-10C16.4FR-P0 0.012" (0.305 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularRoll Length: 16.4 Yards Width, inches: 1Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smoo..
Thickness 330 - 381 microns
13.0 - 15.0 mil
Overall
Arlon R31651R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
Thickness 320 - 380 microns
12.6 - 15.0 mil
Beijing Evergrow Resources ASHRAE HEPA ULPA-K69 Glass Fiber Paper
Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applicat..
Thickness 320 - 380 microns
12.6 - 15.0 mil
Beijing Evergrow Resources ASHRAE HEPA ULPA-K79 Glass Fiber Paper
Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applicat..
Thickness 320 - 380 microns
12.6 - 15.0 mil
Beijing Evergrow Resources ASHRAE HEPA-W19 Glass Fiber Paper
Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applicat..