Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.2 g/10 min @Load 2.16 kg |
8.2 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Relene M60075 Polyethylene Relene M60075 is a High Density Polyethylene grade suitable for injection molding applications where good mechanical properties, gloss, dimensional stability, and good ESCR are required. This grade.. |
|||
Melt Flow | 8.2 g/10 min | 8.2 g/10 min | ISO 1133 |
Solvay Engineered Polymers SEQUEL® 1514 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1514 engineered polyolefin material is designed to provide significantly greater mar resistance than conventional TPOs. SEQUEL® 1514 polyolefin is designed for automotive app.. |
|||
Melt Flow | 8.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® HD-6908 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Stiffness, Good ImpactUses: Crates, Pails, Industrial containers |
|||
Melt Flow | 8.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A; ASTM D1238 |
PolyOne Edgetek® 5209 Black 30 A 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Flow | 8.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A; ASTM D1238 |
PolyOne Edgetek® 5209 Natural 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Flow | 8.2 g/10 min @Load 2.16 kg |
8.2 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Relene L60075 Polyethylene Relene L60075 is UV stabilized. It is available with a recommended service life of more then 5 years L60075 is suitable for applications where articles are exposed to sunlight e.g. soft drink crates.. |
|||
Melt Flow | 8.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® NH-0825 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 8.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® NH-0825 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 8.2 g/10 min @Load 2.16 kg, Temperature 235 °C |
8.2 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238R |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Melt Flow | 8.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escor™ 5000 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5000 is primarily intended for extrusion coating, coextrusion coating, extrusion lamination. Very good adhesion to polar substrates, aluminum foil, metalized films, papers.. |
|||
Melt Flow | 8.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escor™ 6000 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 6000 is primarily intended for extrusion coating and coextrusion coating. Escor 6000 is the high draw down version of Escor 5000. Very low coating weight achievable at hig.. |
|||
Melt Flow | 8.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Melt Flow | 8.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE HD 6909.65 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Melt Flow | 8.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 258 Low Density Polyethylene Resin (European Grade) Product Description: LD 258 is a LDPE extrusion coating grade, having superior organoleptic properties compared to existing standard low odor/off-taste LDPE extrusion coating polymers. The developme.. |