Melt Flow 8.2 g/10 min

@Load 2.16 kg
8.2 g/10 min

@Load 4.76 lb
ASTM D1238
Reliance Industries Relene M60075 Polyethylene
Relene M60075 is a High Density Polyethylene grade suitable for injection molding applications where good mechanical properties, gloss, dimensional stability, and good ESCR are required. This grade..
Melt Flow 8.2 g/10 min
8.2 g/10 min
ISO 1133
Solvay Engineered Polymers SEQUEL® 1514 Engineered Polyolefin  (discontinued **)
Description: SEQUEL® 1514 engineered polyolefin material is designed to provide significantly greater mar resistance than conventional TPOs. SEQUEL® 1514 polyolefin is designed for automotive app..
Melt Flow 8.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene® HD-6908 HDPE, Injection Grade  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Excellent Stiffness, Good ImpactUses: Crates, Pails, Industrial containers
Melt Flow 8.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
PolyOne Edgetek® 5209 Black 30 A 1 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Flow 8.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
PolyOne Edgetek® 5209 Natural 1 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Flow 8.2 g/10 min

@Load 2.16 kg
8.2 g/10 min

@Load 4.76 lb
ASTM D1238
Reliance Industries Relene L60075 Polyethylene
Relene L60075 is UV stabilized. It is available with a recommended service life of more then 5 years L60075 is suitable for applications where articles are exposed to sunlight e.g. soft drink crates..
Melt Flow 8.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
8.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Samsung Cheil Industries Starex® NH-0825 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 8.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
8.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Samsung Cheil Industries Starex® NH-0825 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 8.2 g/10 min

@Load 2.16 kg,
Temperature 235 °C
8.2 g/10 min

@Load 4.76 lb,
Temperature 455 °F
ASTM D1238R
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Melt Flow 8.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escor™ 5000 ExCo Ethylene Acrylic Acid Copolymer Resin
Product Description: Escor 5000 is primarily intended for extrusion coating, coextrusion coating, extrusion lamination. Very good adhesion to polar substrates, aluminum foil, metalized films, papers..
Melt Flow 8.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escor™ 6000 ExCo Ethylene Acrylic Acid Copolymer Resin
Product Description: Escor 6000 is primarily intended for extrusion coating and coextrusion coating. Escor 6000 is the high draw down version of Escor 5000. Very low coating weight achievable at hig..
Melt Flow 8.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin
Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ..
Melt Flow 8.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil HDPE HD 6909.65 High Density Polyethylene Copolymer Resin
Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ..
Melt Flow 8.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LDPE LD 258 Low Density Polyethylene Resin (European Grade)