Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Engineered Polymers SEQUEL® 1514 Engineered Polyolefin  (discontinued **)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers SEQUEL® 1514 Engineered Polyolefin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SEQUEL® 1514 engineered polyolefin material is designed to provide significantly greater mar resistance than conventional TPOs. SEQUEL® 1514 polyolefin is designed for automotive applications that demand low warpage, low CLTE, and excellent scratch and mar resistance. Applications: Integrally colored, unpainted box-top moldings, tailgate liners, and pickup bed trim Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc
0.990 g/cc
ISO 1183
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
as molded; ISO 294
Melt Flow 8.2 g/10 min
8.2 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.0 MPa
2320 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.00 GPa
145 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
38.9 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228
Copyright © lookpolymers.com All Rights Reserved