Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Melt Flow | 6.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Melt Flow | 6.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Melt Flow | 6.6 g/10 min | 6.6 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips MarFlex® 9607XD HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Melt Flow | 6.6 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.6 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 8030 C2 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Melt Flow | 6.6 g/10 min @Load 10.0 kg, Temperature 250 °C |
6.6 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL INT2001 PPE+HIPS (Asia Pacific) PPE+PS Unfilled for Auto Interior |
|||
Melt Flow | 6.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips Marlex® 9006 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Melt Flow | 6.6 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.6 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min15 % Glass fiber reinforcedHigh viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CExtrusionAvailable .. |
|||
Melt Flow | 6.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Entec Hypel® PEHD8/.953 HDPE Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec |
|||
Melt Flow | 6.6 g/10 min | 6.6 g/10 min | ASTM D1238 |
Huntsman Rexell® L3106 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability with good sealing and optical properties.Applications: Blending resin and general purpose packagin.. |
|||
Melt Flow | 6.6 g/10 min | 6.6 g/10 min | ASTM D1238 |
Huntsman Rexell® V3401 Blown Film Extrusion LLDPE
(discontinued **) Ultra linear low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability, toughness, and optics with good sealing properties.Applications: Sealing layer in coextrude.. |