Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers Centrex® 885 Profile Extrusion Grade

Category Polymer , Thermoplastic , ASA Polymer
Manufacturer Diamond and Network Polymers
Trade Name Centrex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers Centrex® 885 Profile Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Centrex 885 resin is a low-gloss ASA (acrylonitrile-styrene-acrylate) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can be coextruded over polyvinyl chloride (PVC).Applications: Typical applications for Centrex 601 resin include exterior siding, window frames and fences. As with any product, use of Centrex 885 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Melt Flow 4.7 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.7 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.8 MPa
2290 psi
chs 0.2 in/min; ASTM D638
Tensile Strength, Yield 26.2 MPa
3800 psi
chs 0.2 in/min; ASTM D638
Flexural Strength 45.5 MPa
6600 psi
chs 0.05 in/min; ASTM D790
Flexural Modulus 1.516 GPa
219.9 ksi
tangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
3.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Impact Test 17.0 J

@Temperature 23.0 °C
12.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
Vicat Softening Point 107 °C

@Load 1.00 kg
225 °F

@Load 2.20 lb
120°C/hr; ASTM D1525
Optical Properties Metric English Comments
Gloss 3.0 %
3.0 %
Extruded Strip; 60°; ASTM D523
Users viewing this material also viewed the following: