Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.00 - 15.0 g/10 min | 2.00 - 15.0 g/10 min | Average value: 8.40 g/10 min Grade Count:5 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Melt Flow | 2.00 - 15.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
2.00 - 15.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB7522 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 - 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1332 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: High Gloss Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 - 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1781 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 5.00 - 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1322 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) Forms: Pellets Features: General PurposeInformation Provided by Teknor Apex |
|||
Melt Flow | 9.00 - 15.0 g/10 min | 9.00 - 15.0 g/10 min | Average value: 12.0 g/10 min Grade Count:4 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |
|||
Melt Flow | 1.00 - 15.0 g/10 min | 1.00 - 15.0 g/10 min | Average value: 8.72 g/10 min Grade Count:73 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |