Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 4.00 - 130 g/10 min
4.00 - 130 g/10 min
Average value: 49.8 g/10 min Grade Count:7
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Melt Flow 4.00 - 130 g/10 min
4.00 - 130 g/10 min
Average value: 42.8 g/10 min Grade Count:13
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Melt Flow 70 - 130 g/10 min

@Load 2.16 kg,
Temperature 190 °C
70 - 130 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
DuPont Elvaloy® HP771 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Melt Flow 8.00 - 130 g/10 min
8.00 - 130 g/10 min
Average value: 64.2 g/10 min Grade Count:9
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma..
Melt Flow 5.00 - 130 g/10 min
5.00 - 130 g/10 min
Average value: 28.1 g/10 min Grade Count:50
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..