Physical Properties Metric English Comments
Melt Flow 105 g/10 min

@Load 2.16 kg,
Temperature 190 °C
105 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 2318 LLDPE Injection Molding Resin  (discontinued **)
Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.Applications: Thin walled container lids and closures.Data provided by the manufacturer.
Melt Flow 105 - 160 g/10 min

@Load 2.16 kg,
Temperature 170 °C
105 - 160 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Lubrizol Advanced Materials PEARLBOND® 122 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 122 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit..
Melt Flow 105 - 160 g/10 min

@Load 2.16 kg,
Temperature 170 °C
105 - 160 g/10 min

@Load 4.76 lb,
Temperature 338 °F
ISO 1133
Lubrizol Advanced Materials PEARLBOND® 522 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 522 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level...
Melt Flow 105 g/10 min
105 g/10 min
ASTM D1238
Total PPC 4920WZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 4920WZ is a nucleated impact copolymer with a Melt Flow index of 105 g/10 min.TOTAL Polypropylene 4920WZ is characterized by excellent stiffness and impact resista..
Melt Flow 105 g/10 min

@Load 2.16 kg,
Temperature 210 °C
105 g/10 min

@Load 4.76 lb,
Temperature 410 °F
cm<sup>3</sup>/10 min; ISO 1133
EMS-Griltech Griltex® D 1502E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melt Flow 105 g/10 min

@Load 2.16 kg,
Temperature 160 °C
105 g/10 min

@Load 4.76 lb,
Temperature 320 °F
cm<sup>3</sup>/10 min; ISO 1133
EMS-Griltech Griltex® D 1539E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melt Flow 105 g/10 min

@Load 2.16 kg
105 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 6.5.
Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2503 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with excellent rigidity. It h..
Melt Flow 105 - 140 g/10 min

@Load 2.16 kg,
Temperature 235 °C
105 - 140 g/10 min

@Load 4.76 lb,
Temperature 455 °F
ASTM D1238
Gromax CCP PBT 1200-211E
Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle..