Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 105 - 160 g/10 min @Load 2.16 kg, Temperature 170 °C |
105 - 160 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 122 Linear Thermoplastic Polyurethane Pearlbond™ 122 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Melt Flow | 105 - 160 g/10 min @Load 2.16 kg, Temperature 170 °C |
105 - 160 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 522 Linear Thermoplastic Polyurethane Pearlbond™ 522 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level... |
|||
Melt Flow | 8.00 - 160 g/10 min | 8.00 - 160 g/10 min | Average value: 39.9 g/10 min Grade Count:22 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |