Polymer Property : Melt Flow = 10.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.100 - 10.0 g/10 min
0.100 - 10.0 g/10 min
Average value: 3.44 g/10 min Grade Count:20
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Melt Flow 0.200 - 10.0 g/10 min
0.200 - 10.0 g/10 min
Average value: 1.86 g/10 min Grade Count:5
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe..
Melt Flow 0.200 - 10.0 g/10 min
0.200 - 10.0 g/10 min
Average value: 3.72 g/10 min Grade Count:14
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Melt Flow 1.00 - 10.0 g/10 min

@Load 10.0 kg,
Temperature 190 °C
1.00 - 10.0 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB3131 Linear Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
Melt Flow 2.50 - 10.0 g/10 min
2.50 - 10.0 g/10 min
Average value: 4.50 g/10 min Grade Count:4
Overview of materials for Polypropylene with Glass Fiber + Bead Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max..
Melt Flow 2.50 - 10.0 g/10 min
2.50 - 10.0 g/10 min
Average value: 5.43 g/10 min Grade Count:7
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..