Physical Properties Metric English Comments
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-1518C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 2.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1538A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 2.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2579A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 2.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2955 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4555A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4565A Thermoplastic Elastomer
Uses: Flexible Grips; Overmolding Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion; Extrusion; Injection Molding Injection ..
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-2635C Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-3260R Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-3954-55 Thermoplastic Elastomer
Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire ..
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-89-P834-B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-93-T0488D-70UJ BLACK Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Uniprene® UN-2640S Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Uniprene® UN-1141A Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Uniprene® UN-7100-45 Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
Melt Flow 2.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ExxonMobil Method
ExxonMobil Escorene® LD 721.IK Film Resin
Escorene Ultra LD 721 is a high vinyl acetate copolymer specialty film resin providing outstanding heat sealability, along with excellent strength properties and clarity.Availability: Latin America,..
Melt Flow 2.50 - 10.0 g/10 min
2.50 - 10.0 g/10 min
Average value: 4.50 g/10 min Grade Count:4
Overview of materials for Polypropylene with Glass Fiber + Bead Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max..
Melt Flow 2.50 - 10.0 g/10 min
2.50 - 10.0 g/10 min
Average value: 5.43 g/10 min Grade Count:7
Overview of materials for Polypropylene, Long Glass Fiber 50%