Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 0.73 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.73 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.73 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Procedure A; ASTM D1238
PolyOne Elastamax™ EG-9190 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun..
Melt Flow 0.73 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.73 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil HDPE AP60-007 High Density Polyethylene Resin
Product Description: AP60-007 is a medium molecular weight distribution high density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear..
Melt Flow 0.73 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.73 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Paxon™ AD60-007 Blow Molding Resin
Product Description: AD60-007 is a medium molecular weight distribution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appear..
Melt Flow 0.73 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.73 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
PolyOne Syncure™ S1027A Polyethylene, Crosslinked (XLPE)
Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Oven Aging, measured on a 100 phr S1027A / 20 phr V0022G system. Deformation, Hot ..
Melt Flow 0.73 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.73 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
PolyOne Syncure™ S1042A Polyethylene, Crosslinked (XLPE)
Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Tensile, Deformation, and Gel measured on a 95 phr S1042A / 5 phr S1000B system; and cured ..
Melt Flow 0.73 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.73 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
PolyOne Syncure™ S1054A Polyethylene, Crosslinked (XLPE)
Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.Oven Aging, Tensile, Elongation, Deformation, Hot Creep, and Gel measured on a 95 phr S1054..
Copyright © lookpolymers.com All Rights Reserved