Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.55 g/10 min @Load 2.16 kg |
0.55 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Relene S42005 Polyethylene Wire and cable High Density Polyethylene grade. Characteristics: excellent processing, superior physical/electrical properties, good environmental stress crack resistance. Applications: recommended .. |
|||
Melt Flow | 0.55 g/10 min | 0.55 g/10 min | ASTM D1238 |
Westlake EB561 6.5% Ethylene Vinyl Acetate Copolymer
(discontinued **) Excellent sealability, excellent impact strength, good optics and enhanced stabilization.Application/UsesFrozen food packagingFresh food packagingIce bagsHeavy duty produce bagsFDA: This material co.. |
|||
Melt Flow | 0.55 g/10 min | 0.55 g/10 min | ASTM D1238 |
Flint Hills P9G1Z-047 Polypropylene Features: Processing stability. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: Thick sheetingInformation Provided by Flint Hills Resources |
|||
Melt Flow | 0.55 g/10 min | 0.55 g/10 min | ASTM-D1238 |
Westlake DA502AA 12% EVA Copolymer (Experimental Product) Westlake DA502AA is a 12% EVA copolymer designed for blown film applications. AA formulation contains no slip and no antiblock. |
|||
Melt Flow | 0.55 g/10 min | 0.55 g/10 min | ASTM-D1238 |
Westlake EB502 12.5% EVA Copolymer Westlake Elevate™ EB502 resin is a fractional melt index 12.5% VA ethylene vinyl acetate copolymer designed for flexible packaging and other films that require excellent toughness and good heat sea.. |
|||
Melt Flow | 0.55 g/10 min | 0.55 g/10 min | ASTM D1238 |
Westlake Elevate™ EF545 4% Ethylene Vinyl Acetate Copolymer Westlake EF545 resin is a 4% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low t.. |
|||
Melt Flow | 0.55 g/10 min | 0.55 g/10 min | ASTM D1238 |
Westlake Elevate™ EF561 6.5% Ethylene Vinyl Acetate Copolymer Westlake EF 561 resin is a fractional melt index 6.5% EVA copolymer designed for ice bags, frozen food bags, and other films that require excellent toughness and good heat sealing characteristics. T.. |
|||
Melt Flow | 0.55 g/10 min | 0.55 g/10 min | ASTM D1238 |
Westlake Elevate™ EF575 7.5% Ethylene Vinyl Acetate Copolymer Westlake EF 575 resin is a fractional melt index 7.5% EVA copolymer designed for ice bags, frozen food bags, and other films that require excellent toughness and good heat sealing characteristics. T.. |
|||
Melt Flow | 0.55 g/10 min | 0.55 g/10 min | ASTM D1238 |
Westlake Hifor Xtreme SC74849 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme Polyethylene SC74849 is a high strength linear low density polyethylene designed for blown film extrusion. This resin contains no slip, no antiblock, and polymer processing aid.. |
|||
Melt Flow | 0.55 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.55 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorSafe™ HE3490-IM HDPE Compound for Injection Molded Pressure Fittings BorSafe™ HE3490-IM is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by .. |
|||
Melt Flow | 0.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 171BA Low Density Polyethylene Resin (European Grade) Product Description: LD 171BA is an LDPE grade, which offers good film rigidity combined with very good optical properties.Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No.. |
|||
Melt Flow | 0.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GM5240PR HDPE High Density Extrusion Polyethylene GM5240PR is a high-density polyethylene compound specially developed for the manufacturing of pipes, underground conduits, and steel pipe coating. This resin is produced with bimodal technology and .. |
|||
Melt Flow | 0.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Coextruded film for automatic packaging (FFS). Information provided by Braskem |
|||
Melt Flow | 0.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem LQ 0518/30 LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Heavy duty bags; shrink film. Information provided by Braskem |
|||
Melt Flow | 0.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer Pluris 9300 is a Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conventional .. |
|||
Melt Flow | 0.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem Pluris 9310 LLDPE Blown Film Extrusion Polyethylene Quatropolymer Pluris 9310 is a Braskem Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conve.. |