Material Notes:
Westlake EF 561 resin is a fractional melt index 6.5% EVA copolymer designed for ice bags, frozen food bags, and other films that require excellent toughness and good heat sealing characteristics. This Kosher compliant resin has excellent low temperature brittleness properties.Application/UsesFrozen food packagingFresh food packagingIce bagsHeavy duty produce bagsFDA: This material complies with FDA regulations in 21 CFR, section 177.1350. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Vinyl Acetate Content 6.5 %
6.5 %
Thickness 31.8 microns
1.25 mil
Melt Flow 0.55 g/10 min
0.55 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 380 %
380 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Dart Drop 18.9 g/micron
480 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 24.1 MPa
3500 psi
ASTM D882
Film Tensile Strength at Break, TD 25.5 MPa
3700 psi
ASTM D882
1% Secant Modulus, MD 103 MPa
15000 psi
ASTM D882
1% Secant Modulus, TD 110 MPa
16000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 4.8 %
4.8 %
ASTM D1003
Gloss 74 %
74 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
with BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film
Region US & Canada
Bamberger Polymers Distribution