Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.500 - 0.700 g/cc | 0.0181 - 0.0253 lb/in³ | ISO 60 |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
Apparent Bulk Density | 0.500 - 0.700 g/cc | 0.0181 - 0.0253 lb/in³ | ISO 60 |
Raschig Group MELOPLAS® 150 MF Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr.. |
|||
Apparent Bulk Density | 0.500 - 0.820 g/cc | 0.0181 - 0.0296 lb/in³ | Average value: 0.663 g/cc Grade Count:6 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | DIN 53 466 |
3M Dyneon™ TF 2072 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 50; Max is 3000. Average particle size 500 µm. Used for wire/cable insulation, 'spaghetti tubing' production.Dyneon offers a family .. |
|||
Apparent Bulk Density | 0.500 - 0.670 g/cc | 0.0181 - 0.0242 lb/in³ | Average value: 0.549 g/cc Grade Count:8 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |
|||
Apparent Bulk Density | 0.500 - 0.680 g/cc | 0.0181 - 0.0246 lb/in³ | Average value: 0.586 g/cc Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Plenco 304 Black Impact Grade Woodflour/Cellulose Filled Phenolic Molding Compound
(discontinued **) Plaslok 304 is a two-stage, woodflour and cellulose-filled phenolic molding compound having improved impact strength. It is suitable for automatic molding, and is recommended for thin-walled parts .. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Plenco 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Plenco 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Plenco 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Plaslok 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 308 is a two-stage, mineral and flock.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Plaslok 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Plaslok 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | Tap density |
Momentive Performance Materials HCPL Boron Nitride (BN) Powder All Grade HCP powders are high purity, fine (99%, -325 mesh), hexagonal Boron Nitride (BN). All exhibit the unique properties of BN in a form readily used in many advanced materials and processes. .. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
Lucobit Lucobit® 1210A Ethylene Copolymer Bitumen Lucobit 1210A is a mixture of ethylene copolymers and special bitumen. Addition of Lucobit to bitumen increases its viscosity and broadens the range of plasticity.Lucobit 1210A in asphalt mixtures .. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
Lucobit Lucolast® 7010 Ethylene Butyl Acrylate Asphalt Additive Lucolast® 7010 is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Addition of Lucolast 7010 to bitumen increases its viscosity, broadens the range of plasticit.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Solvay Specialty Polymers Catalyst CT/2-HP Polyolefin Catalyst CT/2-HP is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® and Polidiemme® series.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Solvay Specialty Polymers Catalyst CT/2-HP UV Polyolefin Catalyst CT/2-HP UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Cogegum® and Polidiemme® ser.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ISO 60 |
SolVin 264GC Polyvinyl Chloride General Purpose - Rigid or Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized, semi-rigid and rigid profiles
- plasticized and rigid pipes
- rigid "pressure" pipes
Injection molding : plasticized and se.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ISO 60 |
SolVin 550GA Copolymer of Vinyl Chloride and Vinyl Acetate Made by suspension polymerization.
APPLICATIONS
Calendering : semi-rigid floor coverings
Lining : fabrics, felts and cardboardInformation provided by SolVin. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 31906 Phenolic, Injection Grade Durez 31906 Black Phenolic is an asbestos free, medium impact, molding compound. It is designed for applications where additional mechanical strength is required.Information provided by Sumitomo Ba.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
Tipco Megabatch® UV 1006 LDPE based UV Stabilizer Masterbatch 15% UV Stabilizer & UV Absorber Masterbatch in LDPE baseApplications: Greenhouse FilmsProcessing: Wide-Width Film ExtrusionInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | TRM-37 |
Tipco Tipcolene® UV 1006 - Combination of UV Stabilizer & UV Absorber Masterbatch with 15% UV & Anti-Oxidants in LDPE |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | TRM-37 |
Tipco Tipcolite® THD 321 Phenolic Compound, Wood Flour & Cellulose, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Wood Flour & CelluloseApplications: Switchgear, HRC FusesProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industries Lt.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | Tap density |
Momentive Performance Materials HCV Boron Nitride (BN) Powder Grade HCV is a 95%, -325 mesh hexagonal Boron Nitride (BN) powder exhibiting the unique properties of BN in a form readily used in the production of many advanced materials. Grade HCV is an initial .. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D4894 |
Solvay Specialty Polymers Algoflon® 15GL PTFE; Glass Fiber Filled
(discontinued **) Data provided by the manufacturer.15 wt.% Glass Fiber. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almos.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Plaslok 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 302 is a two-stage, woodflour and flo.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Plaslok 304 Black Impact Grade Woodflour/Cellulose Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 304 is a two-stage, woodflour and cel.. |
|||
Apparent Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | ASTM D1895 |
Plaslok 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 308 is a two-stage, mineral and flock.. |