Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.500 - 0.820 g/cc | 0.0181 - 0.0296 lb/in³ | Average value: 0.663 g/cc Grade Count:6 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |